430 Stainless Steel Round Bar | Flat Bar

430 Stainless Steel Round Bar | Flat Bar

SteelPRO Group is a leading manufacturer and supplier of 304 Stainless Steel Round Bars/Flat Bars in China. We provide:

ASTM A276 430 round bar/flat bar, UNS S30400 round bar/flat bar, 1.4301 round bar/flat bar, 430 stainless steel square/hexagonal/angle/channel bar, 430 stainless steel hot rolled round bar/flat bar, 430 stainless steel cold drawn round bar/flat bar, 430 stainless steel peeled round bar/flat bar, 430 stainless steel galvanized round bar/flat bar, 430 stainless steel ground round bar/flat bar, 430 stainless steel forged round bar/flat bar, 430 stainless steel coated round bar/flat bar, etc.

Standard

ASTM A240, ASTM A276, EN 10088-3, ISO 683-13

Grade

1.4016, 1Cr15, SUS 430, UNS S43000

Length

1m -12m (3.28' – 39.37'), Customized

Diameter

Customized, Round Bar: 0.5mm – 500mm (0.0'' – 19.6'')

Thickness

Customized, Flat Bar: 0.3mm – 120 mm (0.01'' – 4.72'')

Width

Customized, Flat Bar: 3mm – 500 mm (0.12'' – 19.69'')

Surface Finish

2B, 2D, BA, Bead Blasted, Customized, Electropolished, Hairline, Matte, No. 1, NO. 4, No. 8, Polished, Satin

Form

Angle Bar, Channel Bar, Coated Round Bar/Flat Bar, Cold Drawn Round Bar/Flat Bar, Customized, Forged Round Bar/Flat Bar, Ground Round Bar/Flat Bar, Hexagonal Bar, Hot Rolled Round Bar/Flat Bar, Peeled Round Bar/Flat Bar, Polished Round Bar/Flat Bar, Square Bar

430 Stainless Steel Round Bar | Flat Bar

430 Stainless Steel Round Bar | Flat Bar

  • 430 Round Bar: 430 round bar is a circular-shaped stainless steel product, usually cold or hot-rolled. It offers good corrosion resistance and is easily machinable. Known for its formability, it suits various applications, including automotive parts and fasteners. It is also used in structural and decorative components requiring a smooth, round finish.
  • 430 Flat Bar: 430 flat bar is a flat-shaped stainless steel product, often produced through cold rolling. It provides strong corrosion resistance and good formability. This product is widely used in construction, industrial equipment, and kitchenware. Its flat surface makes it ideal for structural supports and flat mounting applications.
Stainless steel rod product

Business Terms

Business Terms

Terms Specification
Minimum Order Quantity: 5 Tons
Price: To be negotiated
Packaging Details:
As Requested
Delivery Time: Within 7-10 Working Days
Payment Terms: T/T, L/C, Credit Card
Supply Ability: 100000 Tons per month
Certification: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Export To:
United States, Canada, India, Australia, Indonesia, Malaysia, New Zealand, South Africa, United Kingdom, Czech Republic, Germany, Russian Federation, Singapore, Afghanistan, Brazil, Poland, Korea, etc.

Chemical Composition

Chemical Composition

ElementCarbon, CChromium, CrIron, FeManganese, MnPhosphorus, PSulfur, SSilicon, Si
Wt. %≤ 0.1214 – 1879 – 87≤ 1≤ 0.04≤ 0.03≤ 1

Mechanical Properties

Mechanical Properties

PropertyMetricImperial
Tensile Strength, Ultimate517 MPa75 ksi
Yield Strength (at 0.2% offset)345 MPa50 ksi
Rockwell Hardness (B)8585
Elongation at Break25% (in 50 mm)25% (in 2”)
Young’s Modulus200 GPa29 msi

Heat Treatment

Heat Treatment

Common heat treatment processes of ss 430 round bars/flat bars:

  1. Annealing
    • Temperature: 760-815°C (1400-1500°F)
    • Process: Heat slowly and cool in air to relieve internal stress and improve ductility.
  2. Stress Relieving
    • Temperature: 200-300°C (390-570°F)
    • Process: Heat and air-cool to reduce residual stress after machining or forming.

Note: 430 stainless steel cannot be hardened by heat treatment due to its ferritic structure.

Characteristics

Characteristics

  • Strong resistance to oxidation, ideal for long-term applications.
  • High durability ensures a longer lifespan in various uses.
  • Excellent dimensional stability in both round and flat forms.
  • Easy to machine and process, suitable for complex parts.
  • Smooth surface finish supports aesthetic and decorative uses.

Our Service

Our Service

1.Welding

2.Metal Fabrication

3.CNC Machining

4.Lathe

5.Forming

6.OEM/ODM

7.Quenching 

8.Tempering

UT And Hardness Testing

UT And Hardness Testing

UT And Hardness Testing Info

Surface Finish

Surface Finish

Packing

Packing

At SteelPRO Group, we understand the importance of delivering your goods in pristine condition. That’s why we prioritize robust packing solutions to prevent any damage before your shipment arrives. We offer a range of packing methods and customization options to meet your specific needs. Trust us to handle your products with the utmost care and professionalism.

We provide the following packing options (but not limited to these) based on different conditions:

  • Wooden Crates
  • Cardboard Cartons
  • Stretch-Wrapped Pallets
  • Hexagonal Wire Bundles
  • Tubular Protective Sleeves
  • Custom Packaging
  • Plastic Reels
  • Shrink-Wrapped Bundles
  • Bulk Packaging
  • Reel-in-a-Box
  • Custom Packaging
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing

Why Choose Us

Why Choose Us

Stainless steel round bar product factory

SteelPRO Group is a leading manufacturer and solutions provider of specialty steel. We are dedicated to delivering tailored, high-quality solutions across diverse industries. With a commitment to 100% quality assurance, we partner with our clients for mutual growth and success. Trust us to provide the expertise and reliability you need for your critical applications.

Choose us as your trusted partner, and you will get:

  • 17+ Years of Manufacturing Experience
  • 1M+ Tons Annual Capacity
  • 100% Quality Promise
  • Factory Direct Sales Price
  • Complete Specifications & Ample Storage
  • Prompt Delivery
  • Customized Solutions
Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13