420 Stainless Steel Round Bar

420 Stainless Steel Round Bar

SteelPRO Group is a reliable China 420 Stainless Steel Round Bar supplier:

We offer 420 hot rolled round bars, 420 cold rolled round bars, 420 annealed round bars, 420 pickled round bars, 420 polished round bars, 420 forged round bars, 420 turned round bars, 420 precision round bars, and 420 flat bars. We provide customizable processing methods such as cutting, bending, welding, drilling, turning, polishing, grinding, heat treatment, threading, and shearing.

Standard

ASTM A276

Grade

1.4021, 2Cr13, SUS420J2

Length

6000 mm (236.22 in) to 12000 mm (472.44 in), Customized

Diameter

10 mm (0.39 in) to 500 mm (19.69 in), Customized

Surface Finish

Black, Bright, Brushed, Ground, Matte, Mirror, Pickled, Polished, Sandblasted, Smooth

Technique

Annealed, Cold Drawn, Forged, Heat Treated, Hot Rolled, Machined, Pickled, Turned

Shape

Flat, Hexagonal, Hollow, Rectangular, Round, Square, Tapered, Threaded

Form

Annealed Round Bar, Cold drawn round bar and rod, Forged Round Bar, Hot rolled round bar and rod, Machined round bar, Pickled Round Bar, Polished Round Bar, Turned round bar

420 Stainless Steel Round Bar

420 Stainless Steel Round Bar

420 Stainless Steel Round Bar is a type of martensitic stainless steel, available in various diameters and lengths. It has high hardness, good corrosion resistance, strong wear resistance, and is easy to machine. Common applications include knife blades, surgical instruments, pump shafts, valve components, automotive parts.
stainless-steel_bar_rod

Business Terms

Business Terms

Terms Specification
Minimum Order Quantity: 5 Tons
Price: To be negotiated
Packaging Details:
As Requested
Delivery Time: Within 7-10 Working Days
Payment Terms: T/T, L/C, Credit Card
Supply Ability: 100000 Tons per month
Certification: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Export To:
United States, Korea, Russian Federation, India, Mexico, Afghanistan, Albania, Algeria, American Samoa, Andorra, Angola, Anguilla, Antigua And Barbuda, Argentina, Armenia, Australia, Austria, Azerbaijan, Bahamas, Bahrain, Bangladesh, Belarus, Belgium, Belize, Benin, Bhutan, Bolivia, Bosnia And Herzegovina, Botswana, Brazil, Brunei Darussalam, Bulgaria, Burkina Faso, Burundi, Cambodia, Cameroon, Cape Verde, Central African Republic, Chad, Chile, Colombia, Congo, Congo, Democratic Republic, Cook Islands, etc.

Chemical Compositions

Chemical Compositions

lementCarbon (C)Chromium (Cr)Manganese (Mn)Silicon (Si)Phosphorus (P)Sulfur (S)Nickel (Ni)Nitrogen (N)Iron (Fe)
Content (%)0.15% – 0.40%12.0% – 14.0%1.0% max1.0% max0.04% max0.03% max0.75% max0.10% max\

Mechanical Properties

Mechanical Properties

PropertiesMetric UnitImperial Unit
Tensile Strength655 – 860 MPa95 – 125 ksi
Yield Strength450 MPa65 ksi
Vickers Hardness230 – 270 HV230 – 270 HV
Brinell Hardness200 – 250 HB200 – 250 HB
Rockwell Hardness50 – 56 HRC50 – 56 HRC
Elongation20%20%
Elastic Modulus200 GPa29 x 10^6 psi

Heat Treatment

Heat Treatment

  1. Annealing
    • Temperature: 840-900°C
    • Process: Slow cooling in the furnace
  2. Hardening
    • Temperature: 980-1035°C
    • Process: Quenching in oil or air
  3. Low Tempering
    • Temperature: 150-370°C (Low Temper)
    • Process: For high hardness, slow cooling in air
  4. High Tempering
    • Temperature: 370-425°C (High Temper)
    • Process: For improved toughness, slow cooling in air
  5. Stress Relieving
    • Temperature: 150-370°C
    • Process: Slow cooling in air
  6. Sub-Critical Annealing
    • Temperature: less common
    • Process: less common

Characteristic

Characteristic

Here are the characteristics of 420 Stainless Steel Round Bar:

  • Corrosion Resistance: Moderate resistance to corrosion in mild environments.
  • High Hardness: Can be heat treated to achieve high hardness levels.
  • Good Machinability: Easily machined in its annealed condition.
  • Wear Resistance: Provides good wear resistance when hardened.
  • Magnetic: Fully magnetic in all conditions.
  • Weldability: Limited weldability due to its high carbon content.
Stainless steel machine parts

Our Service

Our Service

1.Welding

2.Metal Fabrication

3.CNC Machining

4.Lathe

5.Forming

6.OEM/ODM

7.Quenching 

8.Tempering

UT And Hardness Testing

UT And Hardness Testing

UT And Hardness Testing Info

Surface Finish

Surface Finish

Packing

Packing

  • Durable Packaging Materials: We use high-strength materials like wooden crates and steel straps to prevent damage during transport.
  • Corrosion Protection: Each bar is wrapped in moisture-resistant materials to prevent corrosion during shipping.
  • Custom Sizing: Bars are packed according to the specific length and size requirements to ensure safe and efficient delivery.
  • Labeling and Documentation: Clear labeling and detailed documentation ensure easy identification and handling upon arrival.
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing
stainless steel bars packing

Why Choose Us

Why Choose Us

Stainless steel round bar product factory

SteelPRO Group is a Manufacturer and solutions provider for specialty steel, offering custom services and 100% quality assurance!

Choose us and we can offer you:

  • Ample Stock: Large inventory with custom services. Includes special sizes, surface finishes, and processing services.
  • Global Coverage: A global supply chain and service network to meet the needs of international customers.
  • Quick Response: Fast response within 24 hours for quotations, and professional technical support and after-sales service. Lifetime warranty.
  • Compliance and Certification: Products meet ASTM standards, with SGS or TUV certificates. Each package is labeled for easy identification.
  • Diverse Shipping Options: Choose from FOB, CFR, and CIF shipping methods. Select the best terms to optimize costs and ensure safety.
Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13