SteelPRO Group is a reliable 420 Stainless Steel Sheet supplier from China:
We offer 420 hot rolled sheet, 420 cold rolled sheet, 420 annealed sheet, 420 pickled sheet, 420 perforated sheet, 420 polished sheet, 420 brushed sheet, 420 embossed sheet. We provide customizable processing methods such as cutting, bending, welding, drilling, stamping, polishing, grinding, heat treatment, shearing, and punching.
| Standard | ASTM A240 |
|---|---|
| Grade | 1.4021, 2Cr13, SUS420J1 |
| Length | 6000 mm (236.22 in) to 12000 mm (472.44 in), Customized |
| Width | 1000 mm (39.37 in) to 2000 mm (78.74 in), Customized |
| Thickness | 0.5 mm (0.02 in) to 50 mm (1.97 in), Customized |
| Surface Finish | 2B, BA, Brushed, Embossed, HL (Hairline), Matte, Mirror, No.1, No.4, No.8, Pickled, Sand Blast |
| Technique | Annealed, Bending, Cold Rolled, Cutting, Drilling, Hot Rolled, Pickling, Polishing, Welding |
| Form | Annealed Sheet, Brushed Sheet, Cold Rolled Sheet, Embossed sheet, Heat-treated sheet and plate, Hot rolled sheet and plate, Perforated sheet, Pickled sheet, Polished sheet, Tempered plate |
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, United Kingdom, Australia, Canada, Germany, India, France, Malaysia, Mexico, Netherlands, New Zealand, Russian Federation, Afghanistan, Albania, Algeria, American Samoa, Andorra, Angola, Anguilla, Antigua And Barbuda, Argentina, Armenia, Austria, Azerbaijan, Bahamas, Bahrain, Bangladesh, Belarus, Belgium, Belize, Benin, Bhutan, Bolivia, Bosnia And Herzegovina, Botswana, Brazil, Brunei Darussalam, Bulgaria, Burkina Faso, etc.
|
| Element | C (Carbon) | Cr (Chromium) | Mn (Manganese) | Si (Silicon) | P (Phosphorus) | S (Sulfur) | Ni (Nickel) | Iron (Fe) | Iron (Fe) |
|---|---|---|---|---|---|---|---|---|---|
| Content | 0.15% – 0.40% | 12.0% – 14.0% | 1.0% max | 1.0% max | 0.04% max | 0.03% max | 0.75% max | Balance | \ |
| Properties | Metric Unit | Imperial Unit |
|---|---|---|
| Tensile Strength | 655 – 860 MPa | 95 – 125 ksi |
| Yield Strength | 450 MPa | 65 ksi |
| Vickers Hardness | 230 – 270 HV | 230 – 270 HV |
| Brinell Hardness | 200 – 250 HB | 200 – 250 HB |
| Rockwell Hardness | 50 – 56 HRC | 50 – 56 HRC |
| Elongation | 20% | 20% |
| Elastic Modulus | 200 GPa | 29 x 10^6 psi |
Here are the characteristics of 420 Stainless Steel Sheet:
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
SteelPRO Group is a Manufacturer and solutions provider for specialty steel, offering custom services and 100% quality assurance!